Measured, not judged by eye.

Screw and barrel wear is gradual: output falls, melt quality drops and cycle times creep up long before anything breaks. Measuring flight OD and barrel ID shows how much clearance has opened up, and whether repair or replacement is the right call.

Screw repair

  • Flight lands rebuilt by weld overlay and hardfacing, then ground and polished to finished OD
  • Feed, compression and metering sections assessed by measurement, not appearance
  • Screw tips, check rings and seats repaired or replaced as a matched assembly
  • Drive shanks, keyways and threads repaired; bent screws checked for straightness
  • New screws made to the original geometry, copied from a sample or a drawing

Barrel repair

  • Bore measured along its length for wear, taper and bell-mouthing at the feed
  • Honing to clean up light wear where clearance allows
  • Relining with a new wear liner, including bimetallic liners for abrasive materials
  • Feed throat and flange faces re-machined; heater and thermocouple seats checked
  • New barrels made to a sample or drawing when the old one is past relining
Close-up of a polished injection molding screw, bright flights along its length
The finish

Flights ground and polished, the full length.

After the flight lands are rebuilt, the screw is ground to finished diameter and polished so the surface is smooth and bright end to end. That finish restores the clearance to the barrel, cuts down on material hang-up, and helps the screw convey and melt evenly.

The screw is measured and finished with its barrel as a pair, so the set goes back in with the radial clearance set to spec.

Injection molding

Molding sets, same shop as the extrusion work.

The wear and the repair methods are the same trade, so injection molding screws and barrels are quoted and repaired here too: general-purpose and material-specific screws, barrier and mixing designs, and the whole end of the screw: tip, check valve and nozzle.

Send the screw and barrel together where you can. They’re measured as a pair, so the finished clearance is measured, not estimated.

A worn molding set shows up as
  • Longer recovery time, or cushion that won’t hold steady
  • Short shots at settings that used to run
  • Splay and color streaks from an uneven melt
  • Output that no longer matches screw speed
Signs to watch for

Signs of screw and barrel wear.

Wear shows up in the process long before the parts look bad.

  • 01Output fallingOutput no longer matches screw speed: melt is leaking back over the flights.
  • 02Longer recovery or cycle timeThe screw takes longer to melt the same shot or throughput.
  • 03Poor melt qualityUnmelted particles, color streaks, splay or uneven part weight.
  • 04SurgingPressure and output swing, especially on extrusion lines.
  • 05Higher melt temperatureMore shear heat and longer residence as clearances open up.
  • 06Visible flight wearRounded or chipped flight lands, a polished bore, measurable clearance growth.

Not sure what it is? Try the troubleshooter or tell David what the line is doing.

Screw & barrel questions

Before you send the set.

Repair the set, or make new?
It depends on measured wear. A screw with a sound root and shank can usually be reflighted and hardfaced; a barrel with wear in one zone can often be relined. If the base metal is cracked, bent or worn past an economical repair, we quote a new one made from your sample, so the geometry stays the same.
What should I send with the screw and barrel?
The screw and barrel as a pair, plus the tip assembly for molding sets. The machine make and model, the material you run, and the symptoms you’re seeing help us set the finished clearance and pick the hardfacing.
Do you work on both extrusion and injection molding equipment?
Yes: extrusion screws and barrels, and injection molding screws, barrels, tips and check valves.
Get a quote

Tell us what’s down.

It goes straight to David. Nameplate photos go by text, one tap after you send.

What needs work?

Takes about a minute. Nothing is sent until you press the button.

Equipment
How urgent? (optional)

Rather text? Text David instead, photos and all. Or call (346) 429-7753. Privacy

Text a nameplate photo
  1. 1David reads itYour request lands with him right away, with the equipment and urgency you picked.
  2. 2Send a nameplate photoAfter you send, one tap opens a text to (346) 429-7753 for the photos.
  3. 3Bring it in, get a straight quoteIt’s torn down and inspected, and you get the price and timing before any work starts.

Line down? Pick “Down now”. Equipment that is down gets priority.

The shop: 6922 La Paseo St, Houston, TX 77087.

Output falling? Get the set measured.

Screws and barrels repaired in Houston. 6922 La Paseo St.

Call or text us at this number and we'll get right back to you. SMS Terms · Privacy